Material Properties Acrylonitrile Butadiene Styrene (ABS) 40% Glass Fiber Filled admin May 20, 2016January 17, 2017 Material Properties for Acrylonitrile Butadiene Styrene (ABS) 40% Glass Fiber Filled Physical specifications of materials. Materials Acrylonitrile Butadiene Styrene (ABS) Description 40% Glass Fiber Filled Density g/cc 1.4275 lb/in^3 0.05155 Hardness Brinell unless specified 110(Rockwell-R) Tensile Strength ultimate Mpa 80 Ksi 11.6 Yield Strength MPa 110 Ksi 15.95 Modulus of Elasticity Gpa 9 10^6 Psi 1.304347824 Poisson’s Ratio %Elongation at break 1.5 %Reduction of area Izod Impact J 0.63 Ft-lb 0.464814 Fracture Toughness Mpa(m)^0.5 Ksi(in)^0.5 Thermal conductivity W/m-K 0.23 Btu/ft-h-F 0.13294797686 Specific Heat Cpacity J/g-K Btu/lb-F Coefficient of thermal expansion 1E-6/K 23 1E-6/F 12.796992471 Electrical Resistivity Ohm-cm 1000000000000000