Material Properties

Aluminum Alloy 7075 T6 Temper

Material Properties for Aluminum Alloy 7075 T6 Temper

Physical specifications of materials.

Materials Aluminum Alloy 7075
  Description T6 Temper
Density g/cc 2.81
  lb/in^3 0.102
Hardness Brinell unless specified 150
Tensile Strength ultimate Mpa 572
  Ksi 82.94
Yield Strength MPa 503
  Ksi 72.935
Modulus of Elasticity Gpa 72
  10^6 Psi 10.434782592
Poisson’s Ratio   0.33
%Elongation at break 11
%Reduction of area
Izod Impact J
  Ft-lb
Fracture Toughness Mpa(m)^0.5 25
  Ksi(in)^0.5 22.5
Thermal conductivity W/m-K 130
  Btu/ft-h-F 75.14450866
Specific Heat Cpacity J/g-K 0.96
  Btu/lb-F 0.2304
Coefficient of thermal expansion 1E-6/K 23.6
  1E-6/F 13.1308270572
Electrical Resistivity Ohm-cm 0.0000055