Material Properties

Nickel-Silver 65-18 (752) Annealed

Material Properties for Nickel-Silver 65-18 (752) Annealed

Physical specifications of materials.

Materials Nickel-Silver 65-18 (752)
  Description Annealed
Density g/cc 8.7
  lb/in^3 0.314
Hardness Brinell unless specified 75
Tensile Strength ultimate Mpa 386
  Ksi 55.97
Yield Strength MPa
  Ksi
Modulus of Elasticity Gpa 124
  10^6 Psi 17.971014464
Poisson’s Ratio   0.33
%Elongation at break 35
%Reduction of area
Izod Impact J
  Ft-lb
Fracture Toughness Mpa(m)^0.5
  Ksi(in)^0.5
Thermal conductivity W/m-K
  Btu/ft-h-F
Specific Heat Cpacity J/g-K
  Btu/lb-F
Coefficient of thermal expansion 1E-6/K 17
  1E-6/F 9.458646609
Electrical Resistivity Ohm-cm 0.000029