Cupronickel 30(715) Hardened

Material Properties for Cupronickel 30(715) Hardened

Physical specifications of materials.

Materials Cupronickel 30(715)
  Description Hardened
Density g/cc 8.92
  lb/in^3 0.322
Hardness Brinell unless specified 147
Tensile Strength ultimate Mpa 517
  Ksi 74.965
Yield Strength MPa
  Ksi
Modulus of Elasticity Gpa 152
  10^6 Psi 22.028985472
Poisson’s Ratio   0.33
%Elongation at break 15
%Reduction of area
Izod Impact J
  Ft-lb
Fracture Toughness Mpa(m)^0.5
  Ksi(in)^0.5
Thermal conductivity W/m-K
  Btu/ft-h-F
Specific Heat Cpacity J/g-K
  Btu/lb-F
Coefficient of thermal expansion 1E-6/K 15.5
  1E-6/F 8.6240601435
Electrical Resistivity Ohm-cm 0.0000375