Material Properties Cartridge Brass, (C26000) H00 Temper admin May 20, 2016 Material Properties for Cartridge Brass, (C26000) H00 Temper Physical specifications of materials. Materials Cartridge Brass, (C26000) Description H00 Temper Density g/cc 8.53 lb/in^3 0.308 Hardness Brinell unless specified 109 Tensile Strength ultimate Mpa 400 Ksi 58 Yield Strength MPa 315 Ksi 45.675 Modulus of Elasticity Gpa 110 10^6 Psi 15.94202896 Poisson’s Ratio 0.375 %Elongation at break 35 %Reduction of area Izod Impact J Ft-lb Fracture Toughness Mpa(m)^0.5 Ksi(in)^0.5 Thermal conductivity W/m-K 120 Btu/ft-h-F 69.36416184 Specific Heat Cpacity J/g-K 0.375 Btu/lb-F 0.09 Coefficient of thermal expansion 1E-6/K 19.9 1E-6/F 11.0721804423 Electrical Resistivity Ohm-cm 0.0000062