Material Properties

Aluminum Alloy 1100 H12 Temper

Material Properties for Aluminum Alloy 1100 H12 Temper

Physical specifications of materials.

Materials Aluminum Alloy 1100
  Description H12 Temper
Density g/cc 2.71
  lb/in^3 0.0979
Hardness Brinell unless specified 28
Tensile Strength ultimate Mpa 110
  Ksi 15.95
Yield Strength MPa 103
  Ksi 14.935
Modulus of Elasticity Gpa 69
  10^6 Psi 9.999999984
Poisson’s Ratio   0.33
%Elongation at break 12
%Reduction of area
Izod Impact J
  Ft-lb
Fracture Toughness Mpa(m)^0.5
  Ksi(in)^0.5
Thermal conductivity W/m-K 220
  Btu/ft-h-F 127.16763004
Specific Heat Cpacity J/g-K 0.904
  Btu/lb-F 0.21696
Coefficient of thermal expansion 1E-6/K 23.6
  1E-6/F 13.1308270572
Electrical Resistivity Ohm-cm 0.000003